Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 72.29 MPa @Strain 2.59 %, Temperature 150 °C |
10480 psi @Strain 2.59 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G50HSLA BK039B Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |