Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 72.1 MPa @Strain 2.60 %, Temperature 23.0 °C |
10500 psi @Strain 2.60 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized High Viscosity Polyamide 66 Zytel E51HSB NC010 is a high molecular weight heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by .. |
|||
Tensile Stress | 72.1 MPa @Strain 8.00 %, Temperature 0.000 °C |
10500 psi @Strain 8.00 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |