Mechanical Properties Metric English Comments
Tensile Stress 4.96 MPa

@Strain 45.79 %,
Temperature 60.0 °C
719 psi

@Strain 45.79 %,
Temperature 140 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers