Mechanical Properties Metric English Comments
Tensile Stress 48.97 MPa

@Strain 1.09 %,
Temperature 40.0 °C
7103 psi

@Strain 1.09 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6  (Unverified Data**)
30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performan..
Tensile Stress 48.97 MPa

@Strain 0.500 %,
Temperature 100 °C
7103 psi

@Strain 0.500 %,
Temperature 212 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® HTN 52G45HSL NC010 Polyphthalamide (PPA)
Zytel® HTN52G45HSL NC010 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provide..