Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.78 MPa @Strain 23.93 %, Temperature 100 °C |
1130 psi @Strain 23.93 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |