Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.61 MPa @Strain 40.16 %, Temperature 100 °C |
1100 psi @Strain 40.16 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.61 MPa @Strain 0.150 %, Temperature 90.0 °C |
1100 psi @Strain 0.150 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35EF NC010 Nylon 66 + Nylon 6
(Unverified Data**) 35% Glass Reinforced Polyamide 66 Developed for Electrical and Electronics ApplicationsZytel 70G35EF NC010 is a 35% glass reinforced polyamide 66 developed for electrical and electronics application.. |
|||
Tensile Stress | 7.61 MPa @Strain 0.150 %, Temperature 90.0 °C |
1100 psi @Strain 0.150 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSL NC010 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSL NC010 is a 35% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform.. |
|||
Tensile Stress | 7.61 MPa @Strain 0.200 %, Temperature -40.0 °C |
1100 psi @Strain 0.200 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® FR7026V0F BK001 Nylon 66
(Unverified Data**) Zytel® FR7026V0F BK001 is a flame retardant heat stabilized polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuP.. |
|||
Tensile Stress | 7.61 MPa @Strain 15.56 %, Temperature 40.0 °C |
1100 psi @Strain 15.56 %, Temperature 104 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET
(Unverified Data**) 47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc.. |