Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.39 MPa @Strain 116.86 %, Temperature 120 °C |
1070 psi @Strain 116.86 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.39 MPa @Strain 101.37 %, Temperature 100 °C |
1070 psi @Strain 101.37 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin.. |