Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.31 MPa @Strain 100 % |
1060 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® D6890 TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Tensile Stress | 7.31 MPa @Strain 100 % |
1060 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3990H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 7.31 MPa @Strain 46.91 %, Temperature 120 °C |
1060 psi @Strain 46.91 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc.. |
|||
Tensile Stress | 7.31 MPa @Strain 100 % |
1060 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ G90A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G90A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 7.31 MPa @Strain 100 % |
1060 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ G90A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G90A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |