Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.00 MPa @Strain 10.0 % |
1020 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET
(Unverified Data**) 47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc.. |
|||
Tensile Stress | 7.00 MPa @Strain 10.0 % |
1020 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.00 MPa @Strain 0.500 %, Time 360000 sec |
1020 psi @Strain 0.500 %, Time 100 hour |
ISO 899-1 |
BASF Ultraform N 2320 003 UNC Q600 POM Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent. |
|||
Tensile Stress | 7.00 - 9.00 MPa @Strain 100 % |
1020 - 1310 psi @Strain 100 % |
TM-019G |
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets Elast-Eon™ 2A is a polyurethane with a 40% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc... |
|||
Tensile Stress | 7.00 - 9.00 MPa @Strain 100 % |
1020 - 1310 psi @Strain 100 % |
TM-019G |
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets Elast-Eon™ 2A is a polyurethane with a 40% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc... |
|||
Tensile Stress | 7.00 - 11.0 MPa @Strain 300 % |
1020 - 1600 psi @Strain 300 % |
TM-019G |
AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets Elast-Eon™ 5-325 is a polyurethane with a 32.5% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in .. |
|||
Tensile Stress | >= 7.00 MPa @Strain 100 % |
>= 1020 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 390A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Tensile Stress | >= 7.00 MPa @Strain 100 % |
>= 1020 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 490A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Stress | 7.00 - 11.0 MPa @Strain 300 % |
1020 - 1600 psi @Strain 300 % |
TM-019G |
AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets Elast-Eon™ 5-325 is a polyurethane with a 32.5% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in .. |