Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 47.48 MPa @Strain 0.900 %, Temperature 80.0 °C |
6886 psi @Strain 0.900 %, Temperature 176 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® LW9330 BK851 PBT
(Unverified Data**) Crastin® LW9330 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |
|||
Tensile Stress | 47.47 MPa @Strain 0.779352 %, Temperature -20.0 °C |
6886 psi @Strain 0.779352 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK612SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK612SF is a 15% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |
|||
Tensile Stress | 47.48 MPa @Strain 0.400 %, Temperature 23.0 °C |
6886 psi @Strain 0.400 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN52G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin that can be molded in water heated m.. |