Mechanical Properties Metric English Comments
Tensile Stress 4.71 MPa

@Strain 300 %
683 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P2875 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 4.71 MPa

@Strain 0.0800 %,
Temperature 90.0 °C
683 psi

@Strain 0.0800 %,
Temperature 194 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66  (Unverified Data**)
Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in..
Tensile Stress 4.71 MPa

@Strain 0.190 %,
Temperature 0.000 °C
683 psi

@Strain 0.190 %,
Temperature 32.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1000 BK385 Nylon 1010
UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight...