Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.58 MPa @Strain 0.400 %, Temperature 100 °C |
664 psi @Strain 0.400 %, Temperature 212 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided .. |
|||
Tensile Stress | 4.58 MPa @Strain 150.4 %, Temperature 100 °C |
664 psi @Strain 150.4 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 4.58 MPa @Strain 72.93 %, Temperature 100 °C |
664 psi @Strain 72.93 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process.. |