Mechanical Properties Metric English Comments
Tensile Stress 4.55 MPa

@Strain 300 %
660 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® C4975 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Stress 4.55 MPa

@Strain 300 %,
Temperature 23.0 °C
660 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ HC MT307 Thermoplastic Elastomer (TPE)
Versaflex™ HC MT307 is an extrudable, autoclavable TPE developed for medical tubing applications in healthcare. New Product. Commercial specifications have not been established. - Autoclavable - Fl..
Tensile Stress 4.55 MPa

@Strain 300 %,
Temperature 23.0 °C
660 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ HC MT317 Thermoplastic Elastomer (TPE)
Versaflex™ HC MT317 is an extrudable, sterilizable TPE developed for medical tubing applications in healthcare. - Autoclavable sterilizable - Flexible - Kink Resistant New product. Commercial speci..
Tensile Stress 4.55 MPa

@Strain 300 %,
Temperature 23.0 °C
660 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7680-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7680-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
Tensile Stress 4.55 MPa

@Strain 300 %,
Temperature 23.0 °C
660 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7680-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7680-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
Tensile Stress 4.55 MPa

@Strain 100 %,
Temperature 23.0 °C
660 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7690-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7690-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
Tensile Stress 4.55 MPa

@Strain 100 %,
Temperature 23.0 °C
660 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7690-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7690-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
Tensile Stress 4.55 MPa

@Strain 59.97 %,
Temperature 120 °C
660 psi

@Strain 59.97 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET  (Unverified Data**)
45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers