Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 43.3 MPa @Strain 0.580 %, Temperature 23.0 °C |
6280 psi @Strain 0.580 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9020FR NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020FR NC010 is a 20% glass fiber reinforced flame retardant polybutylene terephthal.. |
|||
Tensile Stress | 43.3 MPa @Strain 2.60 %, Temperature 60.0 °C |
6280 psi @Strain 2.60 %, Temperature 140 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |