Polymer Property : Tensile Stress = 6157 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 42.45 MPa

@Strain 1.89 %,
Temperature 23.0 °C
6157 psi

@Strain 1.89 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F20 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provi..
Tensile Stress 42.45 MPa

@Strain 1.89 %,
Temperature 23.0 °C
6157 psi

@Strain 1.89 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F20UV WT660 Polybutylene Terephthalate (PBT)
Unreinforced UV Stabilized Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provided..
Tensile Stress 42.45 MPa

@Strain 3.81 %,
Temperature 23.0 °C
6157 psi

@Strain 3.81 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 73M40 NC010 Nylon 6  (Unverified Data**)
40% Mineral Reinforced Polyamide 6 Minlon 73M40 NC010 is a 40% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro..