Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 60.8 MPa @Strain 5.40 %, Temperature 23.0 °C |
8820 psi @Strain 5.40 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |