Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 6.08 MPa @Strain 57.62 %, Temperature 90.0 °C |
882 psi @Strain 57.62 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 6.08 MPa @Strain 33.9 %, Temperature 90.0 °C |
882 psi @Strain 33.9 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers |