Mechanical Properties Metric English Comments
Tensile Stress 4.02 MPa

@Strain 1.78 %,
Temperature 90.0 °C
583 psi

@Strain 1.78 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo..
Tensile Stress 4.02 MPa

@Strain 0.300 %,
Temperature 80.0 °C
583 psi

@Strain 0.300 %,
Temperature 176 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® FR7026V0F NC010 Nylon 66  (Unverified Data**)
Zytel® FR7026V0F NC010 is a flame retardant, heat stabilized, polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by D..
Tensile Stress 4.02 MPa

@Strain 0.0600 %,
Temperature 90.0 °C
583 psi

@Strain 0.0600 %,
Temperature 194 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FE350064 BK544 Polyphthalamide (PPA)  (Unverified Data**)
Carbon Fiber Reinforced Toughened PPA High Performance Polyamide Zytel HTNFE350064 BK544 is a carbon fiber reinforced toughened heat stabilized conductive high performance polyamide resin developed ..
Tensile Stress 4.02 MPa

@Strain 16.82 %,
Temperature 40.0 °C
583 psi

@Strain 16.82 %,
Temperature 104 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers
Tensile Stress 4.02 MPa

@Strain 49.12 %,
Temperature 150 °C
583 psi

@Strain 49.12 %,
Temperature 302 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers