Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 58.58 MPa @Strain 7.15 %, Temperature 180 °C |
8496 psi @Strain 7.15 %, Temperature 356 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)
(Unverified Data**) 60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo.. |