Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 58.02 MPa @Strain 1.20 %, Temperature 23.0 °C |
8415 psi @Strain 1.20 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Polyamide 66Zytel 70G13L NC010 is a 13% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |