Polymer Property : Tensile Stress = 558 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 3.85 MPa

@Strain 300 %,
Temperature 23.0 °C
558 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ HC 2110-57B Thermoplastic Elastomer (TPE)
Versaflex™ HC 2110-57B is a TPE designed for use in the healthcare industry offering low stiction and good compression set. New Product. Commercial specifications have not been established. - Bonds..
Tensile Stress 3.85 MPa

@Strain 100 %
558 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P3868H TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 3.85 MPa

@Strain 0.0400 %,
Temperature -20.0 °C
558 psi

@Strain 0.0400 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 540SUV BK544 Polyethylene Terephthalate (PET)  (Unverified Data**)
40% Glass Reinforced UV Stabilized Polyethylene Terephthalate Developed for Extrusion and Injection Molding Rynite 540SUV BK544 is a 40% glass fiber reinforced UV stabilized modified polyethylene te..