Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 37.9 MPa @Strain 0.240 %, Temperature 40.0 °C |
5500 psi @Strain 0.240 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)
(Unverified Data**) 60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo.. |
|||
Tensile Stress | 37.9 MPa @Strain 0.800 %, Temperature 0.000 °C |
5500 psi @Strain 0.800 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 12T NC010 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T NC010 is a 36% mineral reinforced toughened heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performan.. |