Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 55.58 MPa @Strain 0.920 %, Temperature 40.0 °C |
8061 psi @Strain 0.920 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5330HF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HF is a 30% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |
|||
Tensile Stress | 55.58 MPa @Strain 0.980 %, Temperature 40.0 °C |
8061 psi @Strain 0.980 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9020FR NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020FR NC010 is a 20% glass fiber reinforced flame retardant polybutylene terephthal.. |