Mechanical Properties Metric English Comments
Tensile Stress 37.4 MPa

@Strain 100 %
5420 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P3967H TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 37.4 MPa

@Strain 1.04 %,
Temperature 60.0 °C
5420 psi

@Strain 1.04 %,
Temperature 140 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66
Information provided by DuPont Performance Polymers