Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 37.4 MPa @Strain 100 % |
5420 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3967H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 37.4 MPa @Strain 1.04 %, Temperature 60.0 °C |
5420 psi @Strain 1.04 %, Temperature 140 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |