Mechanical Properties Metric English Comments
Tensile Stress 3.72 MPa

@Strain 100 %,
Temperature 21.0 °C
540 psi

@Strain 100 %,
Temperature 69.8 °F
Die C Flow 2 hr; ASTM D412
PolyOne Versalloy™ HC 9220-70 Thermoplastic Elastomer (TPE)
Versalloy™ HC 9220-70 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr..
Tensile Stress 3.72 MPa

@Strain 300 %
540 psi

@Strain 300 %
ASTM D412
Teknor Apex Telcar® TL-1221A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Stress 3.72 MPa

@Strain 0.180 %,
Temperature -40.0 °C
540 psi

@Strain 0.180 %,
Temperature -40.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1000 BK385 Nylon 1010
UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight...