Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.69 MPa @Strain 0.100 %, Temperature 23.0 °C |
535 psi @Strain 0.100 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® FR7026V0F BK001 Nylon 66
(Unverified Data**) Zytel® FR7026V0F BK001 is a flame retardant heat stabilized polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuP.. |
|||
Tensile Stress | 3.69 MPa @Strain 0.0800 %, Temperature 150 °C |
535 psi @Strain 0.0800 %, Temperature 302 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66
(Unverified Data**) Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in.. |
|||
Tensile Stress | 3.69 MPa @Strain 0.180 %, Temperature -40.0 °C |
535 psi @Strain 0.180 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1000 BK385 Nylon 1010 UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight... |
|||
Tensile Stress | 3.69 MPa @Strain 42.0 %, Temperature 90.0 °C |
535 psi @Strain 42.0 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process.. |