Tensile Stress 53.85 MPa

@Strain 12.08 %,
Temperature -20.0 °C
7810 psi

@Strain 12.08 %,
Temperature -4.00 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1600 NC010 Nylon 1010
Plasticized Toughened UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1600 NC010 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced..