Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 360 MPa @Diameter 55.0 - 100 mm, Strain 0.200 % |
52200 psi @Diameter 2.17 - 3.94 in, Strain 0.200 % |
|
United Cast Bar Unibar 600-3 Continuously Cast Spheroidal Graphite Iron Offers reasonable machinability and excellent surface finish combined with higher wear resistance, strength & heat treatment. Noise and vibration damping are good in this grade.Unibar 600-3 can be .. |