Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 52.66 MPa @Strain 17.4 %, Temperature 23.0 °C |
7638 psi @Strain 17.4 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 153HSL NC010 Nylon 612
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers |