Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 51.34 MPa @Strain 10.19 %, Temperature -20.0 °C |
7446 psi @Strain 10.19 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1600 NC010 Nylon 1010 Plasticized Toughened UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1600 NC010 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced.. |