Mechanical Properties Metric English Comments
Tensile Stress 5.88 MPa

@Strain 0.0500 %,
Temperature 23.0 °C
853 psi

@Strain 0.0500 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)  (Unverified Data**)
60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo..
Tensile Stress 5.88 MPa

@Strain 0.105 %,
Temperature 40.0 °C
853 psi

@Strain 0.105 %,
Temperature 104 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 54G15HSLR BK031 Polyphthalamide (PPA)  (Unverified Data**)
15% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G15HSLR BK031 is a 15% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i..
Tensile Stress 5.88 MPa

@Strain 0.0300 %,
Temperature -20.0 °C
853 psi

@Strain 0.0300 %,
Temperature -4.00 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FE350064 BK544 Polyphthalamide (PPA)  (Unverified Data**)
Carbon Fiber Reinforced Toughened PPA High Performance Polyamide Zytel HTNFE350064 BK544 is a carbon fiber reinforced toughened heat stabilized conductive high performance polyamide resin developed ..