Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | >= 5.86 MPa @Strain 50.0 % |
>= 850 psi @Strain 50.0 % |
ASTM D412 Method A |
Seals Eastern 7042 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |
|||
Tensile Stress | 5.86 MPa @Strain 60.28 %, Temperature 150 °C |
850 psi @Strain 60.28 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |