Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.40 MPa @Strain 5.00 % |
783 psi @Strain 5.00 % |
ISO 527-1/-2 |
DSM Arnitel® PM460-H TPC-ET Injection Molding, Heat Stabilized |
|||
Tensile Stress | 5.40 MPa @Strain 0.400 %, Temperature 90.0 °C |
783 psi @Strain 0.400 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical .. |
|||
Tensile Stress | 5.40 MPa @Temperature 100 °C |
783 psi @Temperature 212 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET
(Unverified Data**) Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio.. |