Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 48.46 MPa @Strain 2.25 %, Temperature 90.0 °C |
7029 psi @Strain 2.25 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 32CG20HSL BK409 Nylon 610
(Unverified Data**) 20% Carbon/Glass Reinforced Renewably Sourced Polyamide 610 Information provided by DuPont Performance Polymers |