Polymer Property : Tensile Stress = 4794 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 33.05 MPa

@Strain 0.900 %,
Temperature 150 °C
4794 psi

@Strain 0.900 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® PLS 95G40DH1T BK261 Nylon 6  (Unverified Data**)
40% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G40DH1T is a 40% GR impact modified PA made with SHIELD technology its superior heatInformation provided by DuPont Performance Polymers
Tensile Stress 33.05 MPa

@Strain 0.900 %,
Temperature 150 °C
4794 psi

@Strain 0.900 %,
Temperature 302 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G40DH1T BK261 Nylon  (Unverified Data**)
Zytel® PLS95G40DH1T is a 40% GR impact modified PA, made with SHIELD technology, its superior heat & oil resistance combined with the "stone impact resistance" makes it ideal choice for use in seve..
Tensile Stress 33.05 MPa

@Strain 3.10 %,
Temperature 150 °C
4794 psi

@Strain 3.10 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 32CG20HSL BK409 Nylon 610  (Unverified Data**)
20% Carbon/Glass Reinforced Renewably Sourced Polyamide 610 Information provided by DuPont Performance Polymers