Polymer Property : Tensile Stress = 47100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 325 MPa

@Strain 2.00 %,
Temperature -40.0 °C
47100 psi

@Strain 2.00 %,
Temperature -40.0 °F
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, Conditioned
Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due..
Tensile Stress 325 MPa

@Strain 2.00 %,
Temperature -40.0 °C
47100 psi

@Strain 2.00 %,
Temperature -40.0 °F
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, DRY
Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due..