Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 325 MPa @Strain 2.00 %, Temperature -40.0 °C |
47100 psi @Strain 2.00 %, Temperature -40.0 °F |
|
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, Conditioned Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due.. |
|||
Tensile Stress | 325 MPa @Strain 2.00 %, Temperature -40.0 °C |
47100 psi @Strain 2.00 %, Temperature -40.0 °F |
|
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, DRY Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due.. |