Polymer Property : Tensile Stress = 42100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 290 MPa

@Strain 2.00 %,
Temperature 0.000 °C
42100 psi

@Strain 2.00 %,
Temperature 32.0 °F
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, DRY
Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due..
Tensile Stress 290 MPa

@Diameter 105 - 200 mm,
Strain 0.200 %
42100 psi

@Diameter 4.13 - 7.87 in,
Strain 0.200 %
United Cast Bar Unibar 500-7 Continuously Cast Spheroidal Graphite Iron
Offers higher wear resistance, strength & heat-treatment response while still possessing good machinability and excellent surface finishes. Noise and vibration damping are good in this grade.Unibar ..
Tensile Stress 290 MPa

@Diameter 205 - 600 mm,
Strain 0.200 %
42100 psi

@Diameter 8.07 - 23.6 in,
Strain 0.200 %
United Cast Bar Unibar 500-7 Continuously Cast Spheroidal Graphite Iron
Offers higher wear resistance, strength & heat-treatment response while still possessing good machinability and excellent surface finishes. Noise and vibration damping are good in this grade.Unibar ..