Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.85 MPa @Strain 100 % |
413 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® D6770 TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Tensile Stress | 2.85 MPa @Strain 0.110 %, Temperature 0.000 °C |
413 psi @Strain 0.110 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1000 BK385 Nylon 1010 UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight... |