Polymer Property : Tensile Stress = 40.94 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 40.94 MPa

@Strain 3.73 %,
Temperature 0.000 °C
5938 psi

@Strain 3.73 %,
Temperature 32.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610  (Unverified Data**)
Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by..
Tensile Stress 40.94 MPa

@Strain 0.800 %,
Temperature 40.0 °C
5938 psi

@Strain 0.800 %,
Temperature 104 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 73M40 NC010 Nylon 6  (Unverified Data**)
40% Mineral Reinforced Polyamide 6 Minlon 73M40 NC010 is a 40% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro..