Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 40.82 MPa @Strain 0.450 %, Temperature 90.0 °C |
5920 psi @Strain 0.450 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G50HSLA BK039B Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |