Mechanical Properties Metric English Comments
Tensile Stress 0.280 MPa

@Strain 300 %
40.6 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® C4907 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Stress 0.280 MPa

@Strain 0.200 %,
Temperature 90.0 °C
40.6 psi

@Strain 0.200 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl..