Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 0.280 MPa @Strain 300 % |
40.6 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® C4907 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Stress | 0.280 MPa @Strain 0.200 %, Temperature 90.0 °C |
40.6 psi @Strain 0.200 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl.. |