Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.88 MPa @Strain 300 % |
708 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® S4465 TPE, PS Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesSporting GoodsInformation from Alliance Polymers & Services, Distributor of Nantong .. |
|||
Tensile Stress | 4.88 MPa @Strain 300 % |
708 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® S4665 TPE, PS Overmold Characteristics: Excellent slip resistanceSoft touchGood weather and heat resistanceEasy processingWide range of hardnessExceptional colorabilityTypical Applications: ConsumerElectronicsHealthcareIn.. |
|||
Tensile Stress | 4.88 MPa @Strain 131.23 %, Temperature 90.0 °C |
708 psi @Strain 131.23 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 4.88 MPa @Strain 0.190 %, Temperature 200 °C |
708 psi @Strain 0.190 %, Temperature 392 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6
(Unverified Data**) Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc.. |
|||
Tensile Stress | 4.88 MPa @Strain 51.02 %, Temperature 120 °C |
708 psi @Strain 51.02 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin.. |