Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.51 MPa @Strain 16.88 %, Temperature 100 °C |
654 psi @Strain 16.88 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 4.51 MPa @Strain 100.37 %, Temperature 90.0 °C |
654 psi @Strain 100.37 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |