Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.36 MPa @Strain 300 % |
632 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P1970 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 4.36 MPa @Strain 7.48 %, Temperature 150 °C |
632 psi @Strain 7.48 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |