Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 25.74 MPa @Strain 0.470 %, Temperature 180 °C |
3733 psi @Strain 0.470 %, Temperature 356 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G43L NC010 Nylon 66
(Unverified Data**) 43% Glass Reinforced Polyamide 66Zytel 70G43L NC010 is a 43% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 25.74 MPa @Strain 11.4 %, Temperature 90.0 °C |
3733 psi @Strain 11.4 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 153HSL NC010 Nylon 612
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers |