Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 370 MPa @Diameter 25.0 - 50.0 mm, Strain 0.200 % |
53700 psi @Diameter 0.984 - 1.97 in, Strain 0.200 % |
|
United Cast Bar Unibar 600-3 Continuously Cast Spheroidal Graphite Iron Offers reasonable machinability and excellent surface finish combined with higher wear resistance, strength & heat treatment. Noise and vibration damping are good in this grade.Unibar 600-3 can be .. |