Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 35.5 MPa @Strain 2.00 %, Temperature 40.0 °C |
5150 psi @Strain 2.00 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani.. |
|||
Tensile Stress | 35.5 MPa @Strain 0.900 %, Temperature -40.0 °C |
5150 psi @Strain 0.900 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 900P BK602 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved ProcessingDelrin 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing t.. |
|||
Tensile Stress | 35.5 MPa @Strain 2.00 %, Temperature 40.0 °C |
5150 psi @Strain 2.00 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b.. |
|||
Tensile Stress | 35.5 MPa @Strain 0.970 %, Temperature 180 °C |
5150 psi @Strain 0.970 %, Temperature 356 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSLX BK357 is a 35% glass fiber reinforced heat stabilized black polyamide 66 for injection molding.Information provided by DuPont Perfor.. |
|||
Tensile Stress | 35.5 MPa @Strain 5.30 %, Temperature 120 °C |
5150 psi @Strain 5.30 %, Temperature 248 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |